(Summary description)Deformation of products of injection molding processing enterprises is a relatively common and difficult problem. Through analysis, we want to solve our social problems. From the perspective of machine adjustment, the feasibility is actually not great. The problem of deformation must be solved from the mold structure design management. The reasons for the specific deformation and the teaching methods for solving are as follows :
The main findings are as follows:
1. When the injection molding conditions cause deformation, reduce the stress by reducing the injection pressure, increasing the mold temperature, making the mold temperature uniform, increasing the resin temperature or using annealing methods.
2. When the bad behavior of demolding causes stress to deform, you can continuously increase the number or area of ​​the push rods, and correct the demolding slope.
3. When the cooling is uneven or the cooling time is insufficient, adjust the cooling method to extend the cooling time. Setting the cooling circuit as close to the deformation as possible can also improve the deformation problem.
4. Due to the deformation caused by molding shrinkage, it is necessary to modify the mold design. Among them, the most important thing is to pay attention to making the product wall thickness consistent. Sometimes, if necessary, the mold must adjust the opposite direction by measuring the deformation of the part.
The above are the four major countermeasures to solve product distortion, have you learned? I hope to help you, and there will be more consultations in the future, and interested friends can pay more attention.

How to solve the problem of deformation in injection molds

(Summary description)Deformation of products of injection molding processing enterprises is a relatively common and difficult problem. Through analysis, we want to solve our social problems. From the perspective of machine adjustment, the feasibility is actually not great. The problem of deformation must be solved from the mold structure design management. The reasons for the specific deformation and the teaching methods for solving are as follows :
The main findings are as follows:
1. When the injection molding conditions cause deformation, reduce the stress by reducing the injection pressure, increasing the mold temperature, making the mold temperature uniform, increasing the resin temperature or using annealing methods.
2. When the bad behavior of demolding causes stress to deform, you can continuously increase the number or area of ​​the push rods, and correct the demolding slope.
3. When the cooling is uneven or the cooling time is insufficient, adjust the cooling method to extend the cooling time. Setting the cooling circuit as close to the deformation as possible can also improve the deformation problem.
4. Due to the deformation caused by molding shrinkage, it is necessary to modify the mold design. Among them, the most important thing is to pay attention to making the product wall thickness consistent. Sometimes, if necessary, the mold must adjust the opposite direction by measuring the deformation of the part.
The above are the four major countermeasures to solve product distortion, have you learned? I hope to help you, and there will be more consultations in the future, and interested friends can pay more attention.

Information

Deformation of products of injection molding processing enterprises is a relatively common and difficult problem. Through analysis, we want to solve our social problems. From the perspective of machine adjustment, the feasibility is actually not great. The problem of deformation must be solved from the mold structure design management. The reasons for the specific deformation and the teaching methods for solving are as follows :
The main findings are as follows:
1. When the injection molding conditions cause deformation, reduce the stress by reducing the injection pressure, increasing the mold temperature, making the mold temperature uniform, increasing the resin temperature or using annealing methods.
2. When the bad behavior of demolding causes stress to deform, you can continuously increase the number or area of ​​the push rods, and correct the demolding slope.
3. When the cooling is uneven or the cooling time is insufficient, adjust the cooling method to extend the cooling time. Setting the cooling circuit as close to the deformation as possible can also improve the deformation problem.
4. Due to the deformation caused by molding shrinkage, it is necessary to modify the mold design. Among them, the most important thing is to pay attention to making the product wall thickness consistent. Sometimes, if necessary, the mold must adjust the opposite direction by measuring the deformation of the part.
The above are the four major countermeasures to solve product distortion, have you learned? I hope to help you, and there will be more consultations in the future, and interested friends can pay more attention.

Keyword:

Scan the QR code to read on your phone

Relevant Information

Chinaplast
中国国际橡塑展
查看详情 白箭头 黑箭头
Arabplast
阿拉伯国际橡塑展
查看详情 白箭头 黑箭头
India Plast
印度国际橡塑展
查看详情 白箭头 黑箭头

CONTACT

US

Taizhou Huangyan Erect Mould Co., Ltd.

台州市黄岩艾瑞克模具有限公司

contact Tel/Wechat/Whatsapp:86-15958693992

contact Company email: sales@erectmould.com

contact Address: No 20, Maofeng Road, Xinqian, Huangyan, Taizhou, Zhejiang, China

contact 地址: 中国浙江台州黄岩新前茂丰路20号

2wm

whats app

这是描述信息

Scan to add wechat

2wm

scan
Into the website

© Taizhou Huangyan Erect Mould Co., Ltd Co., Ltd. All Rights Resserved.   浙ICP备2021022484号  Powered by 300.cn